高放射性核废料地质处置环境中钛处置罐腐蚀研究的进展

, PP. 160-164

Full-Text   Cite this paper   Add to My Lib

Abstract:

References

[1]  He X, No?l J J, Shoesmith D W. Temperature dependence of crevice corrosion initiation on titanium grade-2 [J]. J. Electrochem. Soc., 2002, 149(9): B440
[2]  Mckay P, Mitton D B. An electrochemical investigation of localized corrosion on titanium in chloride environments [J]. Corrosion, 1985, 41(1): 52
[3]  He X, No?l J J, Shoesmith D W. Effects of iron content on microstructure and crevice corrosion of grade-2 titanium [J]. Corrosion, 2004, 60(4): 378
[4]  Tsujikawa S, Kojima Y. Repassivation method to predict long term integrity of low alloy titanium for nuclear waste package [J]. Mater. Res. Soc. Symp. Proc, 1991, 212: 261
[5]  郭永海, 王驹, 刘淑芬等. 高放废物处置库预选区野马泉岩体地下水化学特征 [J]. 原子能科学技术, 2004(38增刊): 143
[6]  阳靖峰. 高放废物地质处置环境下金属处置罐材料的腐蚀行为 [D]. 中国科学院, 2011
[7]  Vicentini B, Sinigaglia D, Taccani G. Crevice corrosion of titanium. Behaviour of galvanic cell between shielded and unshielded titanium in sulphuric acid [J]. Corros. Sci., 1975, 15(12): 479
[8]  AbduIsalam M I, Pickering H W, The effect of crevice-opening dimension on the stability of crevice corrosion for nickel in sulfuric acid [J]. J. Electrochem. Soc., 1998, 145 (7): 2276
[9]  AbduIsalam M I, Pickering H W. Effect of the applied potential on the potential and current distributions within crevices in pure nickel [J]. Corros. Sci., 1999, 41: 351
[10]  Grauman J S. Beta-21S: A New High Strength, Corrosion Resistant Titanium Alloy [A]. Proceedings of the international conference on titanium products and applications [C]. Boulder: TDA, 1990: 290
[11]  Bergman D D, Grauman J S. The detection of crevice corrosion in titanium and its alloys through the use of potential monitoring [A]. Titanium'92 Science and Technology [C]. Warrendale: TMS, 1992: 2193
[12]  Brossia C S, Cragnolion G A. Effect of palladium on the corrosion behavior of titanium [J]. Corros. Sci., 2004, 46(7): 1693
[13]  Kobayashi M, Araya Y, Fujiyama S, et al. Study on crevice corrosion of titanium [A]. Proceedings of the 4th International Conference on Titanium [C]. Warrendale: The Metallurgical Society of AIME, 1980: 2613
[14]  He X, Dunn D S, Csontos A A. Corrosion of similar and dissimilar metal crevices in the engineered barrier system of a potential nuclear waste repository [J]. Electrochim. Acta, 2007, 52: 7556
[15]  褚武扬. 氢损伤和滞后断裂 [M]. 北京: 冶金工业出版社, 1988
[16]  Abdulsalam M I. Crevice corrosion of titanium in high temperature-concentrated chloride environments [J]. J. Mater. Eng. Perform., 2007, 16(6): 736
[17]  Yan L, Ramamurthy S, No?l J J, et al. Hydrogen absorption into alpha titanium in acidic solutions [J]. Electrochim. Acta, 2006, 52: 1169
[18]  伍怀龙, 赵国庆, 周筑颖等. 氘在钛中的扩散行为 [J]. 核技术, 1996, 19(6): 326
[19]  Ogawa T, Yokoyama K, Asaoka K, et al. Hydrogen absorption behavior of beta titanium alloy in acid fluoride solutions [J]. Biomaterials, 2004, 25(12): 2419
[20]  Yokoyama K, Ogawa T, Asaoka K, et al. Hydrogen absorption of titanium in acidic fluoride solutions [J]. Mater. Sci. Eng., 2004, A 384(1-2): 19
[21]  Hirohata Y, Motojima D, Hino T, et al. Suppression of hydrogen absorption to V-4Cr-4Ti alloy by TiO2/TiC coating [J]. J. Nucl. Mater., 2003, 313-316: 172
[22]  Nishimura R, Shirono J, Jonokuchi A. Hydrogen-induced cracking of pure titanium in sulphuric acid and hydrochloric acid solutions using constant load method [J]. Corros. Sci., 2008, 50: 2691
[23]  Roy A K, Spragge M K, Fleming D L, et al. Cracking of titanium alloys under cathodic applied potential [J], Micron, 2001, 32(2): 211
[24]  卞敏, 李英秋, 刘钧等. 高纯金属钛中微量氢的分析方法研究 [J]. 稀有金属与硬质合金, 2009, 37(4): 36
[25]  Blaauw M. Hydrogen precipitation in titanium observed with neutron incoherent scattering and prompt gamma neutron activation analysis [J]. Nucl. Instrum. Methods Phys. Res., Sect., 2003, 505(1-2)A: 20
[26]  Gibbons M R, Richards W J, Shields K. Optimization of neutron tomography for rapid hydrogen concentration inspection of metal castings [J]. Nucl. Instrum. Methods Phys. Res., Sect., 1999, 424(1)A: 53
[27]  尹开锯, 李聪, 邱绍宇等. 核废料包装材料研究现状 [J]. 核动力工程, 2007, 28(2): 76
[28]  王驹, 陈伟明, 苏锐等. 我国高放废物地质处置库场址筛选总体技术思路探讨 [J]. 世界核地质科学, 2011, 28(1): 45
[29]  Bennett D G, Gens R. Overview of European concepts for high-level waste and spent fuel disposal with special reference waste container corrosion [J]. J. Nucl. Mater., 2008, 379: 1
[30]  Féron D, Crusset D, Gras J M. Corrosion issues in nuclear waste disposal [J]. J. Nucl. Mater., 2008, 379: 16
[31]  Johnson L H, Shoesmith D W, Ikeda B M, et al. Lifetimes of titanium and copper containers for the disposal of used nuclear fuel [J]. Mat. Res. Soc. Symp. Proc, 1992, 257: 439
[32]  Shoesmith D W, Hocking W H, Ikeda B M, et al. Application of electrochemical methods in the development of models for fuel dissolution and container corrosion under nuclear waste disposal conditions [J]. Can. J. Chem., 1997, 75: 1566
[33]  Nakayama G,Sakakibara Y, Taniyama Y, et al. The long-term behaviors of passivation and hydride layer of commercial grade pure titanium in TRU waste disposal environments [J]. J. Nucl. Mater., 2008, 379: 174
[34]  Nishimura T, Corrosion resistance of molybdenum-containing titanium alloy for overpack in simulating underground environment [J]. J. Nucl. Mater., 2009, 385(3): 495
[35]  Andresen P L, Gordon G M, Lu S C. The stress-corrosion-cracking model for high-level radioactive-waste packages [J]. JOM-Min. Met. Mat., 2005, 1S: 27
[36]  Griess J C. Crevice corrosion of titanium in aqueous salt solutions [J]. Corrosion, 1968, 24(4): 96
[37]  R. 温斯顿. 里维. 尤利格腐蚀手册 [M]. 北京: 化学工业出版社, 2005
[38]  王健云, 周清木, 秦平刚等. 工业纯钛的缝隙腐蚀探讨 [J]. 化工机械, 2000, 27(3): 135
[39]  Satoh H, Shimogori K, Kamikubo F. The crevice corrosion resistance of some titanium materials [J]. Platinum Met. Rev., 1987, 31(3): 115
[40]  Tsujikawa S, Kojima Y. Crevice corrosion-NaCl concentration map for grade-2 titanium at elevated temperature [J]. Mater. Res. Soc. Symp. Proc, 294, 1993: 311
[41]  Schutz R W. Understanding and preventing crevice corrosion of titanium alloys II [J]. Mater. Performance, 1992, 31(11): 54
[42]  Yan L, No?l J J, Shoesmith D W, Hydrogen absorption into grade-2 titanium during crevice corrosion [J]. Electrochim. Acta, 2011, 56: 1810
[43]  Rajendran N, Nishimura T. Crevice corrosion monitoring of titanium and its alloys using microelectrodes [J]. Mater. Corros., 2007, 58(5): 334