China Foundry  2008 

Prevention of burn-on defect on surface of hydroturbine blade casting of ultra-low-carbon refining stainless steel

Keywords: burn-on defect , ultra-low-carbon martensitic stainless steel , chromium-corundum coatings

Full-Text   Cite this paper   Add to My Lib

Abstract:

The burn-on sand is common surface defect encountered in CO2-cured silicate-bonded sand casting of hydroturbine blade of ultra-low-carbon martensitic stainless steel, its feature, causes and prevention measures are presented in this paper. Experiments showed that the burn-on defect is caused by oxidization of chromium in the molten steel at high temperature and can be effectively eliminated by using chromium-corundum coating.