%0 Journal Article %T 叠氮苯并咪唑偶联剂增强国产芳纶Ⅲ/聚三唑树脂复合材料界面<br>Interfacial reinforcement of domestic aramid fiber Ⅲ/PTA composites using azide-containing benzimidazole coupling agent %A 刘冬冬 %A 扈艳红 %A 张芳芳 %A 顾渊博 %J 复合材料学报 %D 2017 %R 10.13801/j.cnki.fhclxb.20160407.003 %X 通过分子设计制备合成了含叠氮及苯并咪唑双官能团的偶联剂Azido-Benzimidazole(ABI),并考察了新型偶联剂对国产芳纶Ⅲ(DAF-Ⅲ)/聚三唑树脂(PTA)复合材料的界面增强作用。SEM、傅立叶变换衰减全反射红外光谱(ATR-FTIR)及XPS分析表明,ABI通过分子结构中的苯并咪唑基团与DAF-Ⅲ纤维形成分子间氢键,能够作用到DAF-Ⅲ上。FTIR及DSC分析表明,ABI中的叠氮基团与PTA树脂中的炔基发生反应,生成三唑环参与了PTA树脂的固化。经2.1wt% ABI处理后,DAF-Ⅲ/PTA树脂复合材料层间剪切强度(ILSS)和弯曲强度分别较未处理时提高了62.0%和43.7%。 A new type of coupling agent Azido-Benzimidazole (ABI) containing benzimidazole and azide groups was designed and prepared in this study.And ABI was added into the domestic aramid fiber Ⅲ(DAF-Ⅲ)/polytriazole (PTA) composites to reinforce their interfacial properties.The results of SEM,Attenuated Total internal Reflectance Fourier Transform Infrared Spectroscopy (ATR-FTIR) and XPS show that ABI can bond with the fiber by intermolecular hydrogen;FTIR and DSC results indicate that the azide group in ABI can react with alkynyl in PTA and take part in the curing process synchronously.The mechanical performances of DAF-Ⅲ/PTA composite are improved greatly after ABI modification.The Inter Laminar Shear Strength (ILSS) and flexural strength increase by 62.0% and 43.7% respectively after 2.1wt% ABI treatment compared with those of untreated composites. 特种功能高分子材料及相关技术教育部重点试验室(B类)开放基金上海市重点学科项目编号(B502) %K 国产芳纶Ⅲ %K 聚三唑树脂 %K 苯并咪唑 %K 叠氮 %K 偶联剂 %K 界面增强< %K br> %K domestic aramid fiber Ⅲ (DAF-Ⅲ) %K polytriazole (PTA) %K benzimidazole %K azide group %K coupling agent %K interfacial properties %U http://fhclxb.buaa.edu.cn/CN/abstract/abstract13549.shtml