%0 Journal Article %T 硬脂酸改性β-磷酸三钙及其复合材料机械性能研究 %A 陈赛 %A 马凤仓 %A 耿芳 %A 刘平 %A 刘新宽 %A 李伟 %J 材料科学与工业 %D 2016 %R 10.11951/j.issn.1005-0299.20160111 %X 为了提高β-磷酸三钙(β-TCP)复合材料的机械性能,采用硬脂酸(C17H25COOH)对β-TCP表面进行改性处理,研究了β-TCP与C17H25COOH的界面作用机理.利用透射电镜、傅里叶红外光谱、热重分析等技术分别对改性前后β-TCP的颗粒形貌、组分和表面—OH基团进行了表征,研究了改性β-TCP/聚左旋乳酸(PLLA)复合材料的机械性能,并利用扫描电镜观察了复合材料断面形貌.研究表明:硬脂酸包覆在β-TCP表面,改性后β-TCP粉末具有一定的疏水性, 硬脂酸的H+可以与β-TCP中的PO43-的一个O发生质子化反应形成—OH.改性β-TCP/PLLA复合材料的机械性能相比改性前有明显提高,改性后的β-TCP微粒在PLLA中分散均匀,两者结合紧密.</br>To improve the mechanical properties of beta-tricalcium phosphate(β-TCP) composite, β-TCP was modified using stearic acid (C17H25COOH). The mechanism of interfacial interactions between β-TCP particles and stearic acid was studied. The morphology, component and —OH of β-TCP′s surface before and after surface modification were studied by TEM, FTIR, TG, DTG and XPS. The mechanical properties and the morphology of fracture surface of the modified β-TCP/poly-L-lactic acid(PLLA) composite were also studied. The results indicate that the stearic acid coats on the surface of β-TCP particles, and the modified β-TCP powder is hydrophobic. H+ of stearic acid could produce protonation reaction with O of β-TCP′s PO43- and then generates —OH. Surface modification of β-TCP particles could improve the mechanical strengths of the β-TCP/PLLA composites dramatically. The β-TCP particles with surface modification distribute in the PLLA matrix uniformly and combine with the PLLA matrix closely. %K β-磷酸三钙 %K 硬脂酸 %K 表面改性 %K 复合材料 %K 机械性能< %K /br> %K β-tricalcium %K phosphate %K stearic %K acid %K surface %K modification %K composites %K mechanical %K properties %U http://hit.alljournals.cn/mst_cn/ch/reader/view_abstract.aspx?file_no=20160111&flag=1