%T CAVITATION AND RESIDUAL STRENGTH OF AS-WARM ROLLED Al-Li-Cu-Mg-Zr ALLOY AFTER SUPERPLASTIC DEFORMATION
温轧态Al—Li—Cu—Mg—Zr合金超塑变形后空洞行为与残余强度的研究
%A LIU Qing
%A LIU Zhengang
%A YAO Mei University of Science
%A Technology Beijing Harbin Institute of Technology
%A
刘庆
%A 刘振纲
%A 姚枚
%J 金属学报
%D 1993
%I
%X The residual strength and relation to the cavitation of as-warm rolled Al-Li-Cu-Mg-Zr alloy have been investigated after superplastic deformation under differ- ent tensile conditions. Under certain extent of strain, the specimen deformed at a high strain rate has less cavity and higher residual strength than that at low strain rate. While deformation to a large strain, the specimen deformed under test at strain rates of two-stage, i.e., at a quick one first and slow down afterward, has less cavity and higher residual strength in comparison with that of a single stage. The relationship among residual strength, cavitation and superplastic tensile conditions has been discussed by considering the deformation-in- duced continuous recrystallization occurred during the initial stage of superplastic deformation.
%K Al-Li-Cu-Mg-Zr alloy
%K superplastic deformation
%K residual strength
%K cavitation
铝锂合金
%K 控制轧制
%K 空洞
%K 强度
%U http://www.alljournals.cn/get_abstract_url.aspx?pcid=5B3AB970F71A803DEACDC0559115BFCF0A068CD97DD29835&cid=AB188D3B70B071C57EB64E395D864ECE&jid=B061E1135F1CBDEE96CD96C109FEAD65&aid=9D6A0706ECC10733EBD065602FA0DA4E&yid=D418FDC97F7C2EBA&vid=771469D9D58C34FF&iid=9CF7A0430CBB2DFD&sid=C5154311167311FE&eid=340AC2BF8E7AB4FD&journal_id=0412-1961&journal_name=金属学报&referenced_num=0&reference_num=6