%0 Journal Article
%T Influence of Liquid Ceramic Additive on Binding of Heavy Metal During the Vitrification of Fly Ash from Municipal Solid Waste Incinerator
LC添加剂对垃圾焚烧飞灰熔融过程重金属迁移特性的影响
%A LI Run-dong
%A NIE Yong-feng
%A LI Ai-min
%A WANG Lei
%A CHI Yong
%A CEN Ke-fa
%A
李润东
%A 聂永丰
%A 李爱民
%A 王雷
%A 池涌
%A 岑可法
%J 环境科学
%D 2004
%I
%X Vitrification process can effectively control the leachability of heavy metals in fly ash generated from municipal solid waste incinerator(MWSI).The use of liquid ceramic(LC)additive as a heavy metal chemical stabilization agent was evaluated for MSWI fly ash. The residuals of chromium,lead and zinc in slag increase by different degree with liquid ceramic additive less than 10%.The volatilization of Cr and Zn occurs after 61 minute with 10% addition of LC, and the binding efficiency of Cr decreases with increasing of melting temperature. The results indicate that the binding efficiency of heavy metals was affected greatly by LC additive and showed significant differences according to type of heavy metal during melting process. The short melting time (no longer than 33min) is useful to obtain high binding efficiency of heavy metals.
%K 垃圾焚烧飞灰
%K 熔融
%K 重金属
%K 迁移
%U http://www.alljournals.cn/get_abstract_url.aspx?pcid=3FF3ABA7486768130C3FF830376F43B398E0C97F0FF2DD53&cid=A7CA601309F5FED03C078BCE383971DC&jid=64CD0AA99DD39F69401C615B85F123EF&aid=A65A8F264CA12D09&yid=D0E58B75BFD8E51C&vid=C5154311167311FE&iid=94C357A881DFC066&sid=BBF7D98F9BEDEC74&eid=73579BC9CFB2D787&journal_id=0250-3301&journal_name=环境科学&referenced_num=6&reference_num=9