%0 Journal Article %T Recovery of Gold from Gold-leaching Acidic Thiourea Solution by P507 Extraction and Na2SO3 Stripping
P507从酸性硫脲浸金液中回收金 %A ZHU Ping %A GU Guo-bang %A JIA Bao-qiong %A
朱萍,古国榜,贾宝琼 %J 过程工程学报 %D 2002 %I %X The performance using P507 to extract gold from gold-leaching acidic thiourea solution was investigated. Gold was extracted by P507 of 1.65 mol/L in kerosene under the conditions of H2SO4 concentration 0.335 mol/L, phase ratio 1:1 and time of contact 5 min. The percentage extraction in a single stage reached 99.80%. When 50 g/L Na2SO3 was used for stripping, the percentage stripping in one stage reached 82.45%, and gold was separated from iron by stripping operation. %K gold %K thiourea %K extraction %K P507
酸性硫脲浸金液 %K 回收 %K 金 %K P507 %K 溶剂萃取 %K 萃取剂 %U http://www.alljournals.cn/get_abstract_url.aspx?pcid=5B3AB970F71A803DEACDC0559115BFCF0A068CD97DD29835&cid=3FCF8B1A330466D5&jid=B9EE12934D19905403D996AE65CEEEED&aid=2D24CAADDB794E5E&yid=C3ACC247184A22C1&vid=0B39A22176CE99FB&iid=0B39A22176CE99FB&sid=E22B6B8FE86DD8F9&eid=769BD58726D66E7D&journal_id=1009-606X&journal_name=过程工程学报&referenced_num=2&reference_num=7