%0 Journal Article
%T LABORATORY INVESTIGATION OF THE INITIALLY CORRODED ZINC SURFACES IN AIR CONTAINING SO2
Zn在SO2环境下大气腐蚀初期表面特性研究
%A YAN Chuanwei
%A SHI Zhiming
%A LIN Haichao
%A CAO Chu''''nan
%A
严川伟
%A 史志明
%A 林海潮等
%J 腐蚀科学与防护技术
%D 2000
%I
%X Laboratory expxure of zinc was carried out under the condition of 0.9 x 902 and 90% relative humidity in order to investigate the characteristics of ded surface and its role in initial stage. Scanning electmn microscope (SIN/EDAX), IR microscope were used for the characterisation of ded surfaces. It was found that wer 10 h exposure resulted in a rather uniformly d l ncduls like mrphology with size about I-, which was not kept until local cornion sprouted wer a week mure. The cornion product on locally coded area with porous appearance, was mnposed of needle-shaped crystals. Based on the IR and EDAX, it was infered that the product was Z&Q(OH)6 .5H20. The mechanism of atnmpheric cornion for zinc under the condition is discussed.
%K zinc
%K atmospheric corrosion
%K sulphure dioxide
%K micro-IR
锌
%K 大气腐蚀
%K 二氧化硫
%K 显微红外光谱
%U http://www.alljournals.cn/get_abstract_url.aspx?pcid=5B3AB970F71A803DEACDC0559115BFCF0A068CD97DD29835&cid=AB188D3B70B071C57EB64E395D864ECE&jid=9F6E6EC8BA5BB62698F6640073DDD6E1&aid=B642AAA0D163A0C6&yid=9806D0D4EAA9BED3&vid=59906B3B2830C2C5&iid=38B194292C032A66&sid=70AC2EF7F2065E09&eid=D59111839E7C8BDF&journal_id=1002-6495&journal_name=腐蚀科学与防护技术&referenced_num=3&reference_num=9