%0 Journal Article %T THE POSITRON LIFETIME IN AMORPHOUS NiCrFeSiB ALLOY AFTER HYDROGEN CHARGING
非晶态镍合金渗氢后的正电子寿命谱特征 %A HUANG Weidong %A ZUO Yu %A WEI Long %A WANG Wenhua %A
黄卫东 %A 左禹 %A 魏龙 %A 王文华 %J 腐蚀科学与防护技术 %D 1998 %I %X The positron lifetime in amorphous NiCrFeSiB alloy with and without hydrogen charging was measured to understand the interaction between hydrogen and point defects in amorphous structure. Free volume and vacancy group were found in the alloy as main defects. Hydrogen charging in low current density had little influence on the defect structure. High current density charging resulted in an increase of vacancy group concentration temporarily. However, the stable defect structre recovered after hydrogen escaped from the alloy. %K amorphous alloy %K hydrogen %K positron
非晶态合金 %K 正电子寿命 %K 渗氢 %K 镍合金 %U http://www.alljournals.cn/get_abstract_url.aspx?pcid=5B3AB970F71A803DEACDC0559115BFCF0A068CD97DD29835&cid=AB188D3B70B071C57EB64E395D864ECE&jid=9F6E6EC8BA5BB62698F6640073DDD6E1&aid=0476B6698D65725FA39FD854F78E58C5&yid=8CAA3A429E3EA654&vid=F3090AE9B60B7ED1&iid=CA4FD0336C81A37A&sid=1AE5323881A5ECDC&eid=D997634CFE9B6321&journal_id=1002-6495&journal_name=腐蚀科学与防护技术&referenced_num=0&reference_num=2