%0 Journal Article %T Effect of Y2O3 and Total Oxide Addition on Mechanical Properties of Pressureless Sintered β-SiC %A Gang Wang %A Vladimir DKrstic %A
GangWang %A VladimirD.Krstic %J 材料科学技术学报 %D 2003 %I %X The effect of Y2O3 and the total oxide volume fraction (Y2O3 Al2O3) on density and mechanical properties of low temperature (1770~1940℃) pressureless sintered β-SiC ceramics were presented. The optimum temperature for pressureless sintering of β-SiC was found to be~1850℃ and the optimum content of Y2O3 in the oxides was found to be between 40 and 57 wt pct. The highest sintered density was achieved by adding oxides at 14 vol. pct. Both of the highest strength and fracture toughness were achieved at~14 vol. pct oxide addition and yttria concentrations between 40 and 57 wt pct in the oxides. Hardness, on the other hand, was found to be the highest for samples with 14 vol. pct oxide addition and ~64 wt pct Y2O3 in oxides. %K Y_2O_3 %K SiC %K Mechanical properties %K Sintering
Y2O3 %K 机械性质 %K β-SiC陶瓷 %K 无压烧结 %K 氧化钇 %U http://www.alljournals.cn/get_abstract_url.aspx?pcid=5B3AB970F71A803DEACDC0559115BFCF0A068CD97DD29835&cid=84529CA2B2E519AC&jid=324DC3CAB22330DB19158AE0A9B7BFA5&aid=802B574348F77E74&yid=D43C4A19B2EE3C0A&vid=2A8D03AD8076A2E3&iid=38B194292C032A66&sid=23104246A5FCFCEF&eid=E0F6F365E4766526&journal_id=1005-0302&journal_name=材料科学技术学报&referenced_num=0&reference_num=21