%0 Journal Article %T Laser Welding of TC-1 Titanium Alloy %A Hanbin DU %A Lunji HU %A Xiyuan HU %A Jianhua LIU %A
HanbinDU %A LunjiHU %A XiyuanHU %A JianhuaLIU %J 材料科学技术学报 %D 2003 %I %X The technology of CO2 laser welding and joint properties of titanium alloy were investigated. The problem of molten pool protection was resolved by designing a shielding trailer and a special clamp. Joints with silvery appearance were obtained, which have no pore and crack. In addition, the welding speed could reach 3 m/min for the plate of 1.5 mm thickness being penetrated. The reason of the porosity formation in partial penetration joints is that the keyholes can be easily cut apart in the radial direction, which makes the gas enclosed in the molten pool. The surface oxide of specimens can not affect the porosity formation in welds directly. %K Titanium alloy %K CO2 laser welding %K Porosity formation mechanism
CO2激光焊接 %K 钛合金 %K 多孔性 %K 形成机制 %K 二氧化碳激光焊接 %U http://www.alljournals.cn/get_abstract_url.aspx?pcid=5B3AB970F71A803DEACDC0559115BFCF0A068CD97DD29835&cid=84529CA2B2E519AC&jid=324DC3CAB22330DB19158AE0A9B7BFA5&aid=11209736B98A9E65&yid=D43C4A19B2EE3C0A&vid=2A8D03AD8076A2E3&iid=94C357A881DFC066&sid=D93AD940782892D0&eid=A94616C4391AA5EF&journal_id=1005-0302&journal_name=材料科学技术学报&referenced_num=0&reference_num=3