%0 Journal Article %T DIFFUSIVITY OF HYDROGEN IN STEELS AT LOW TEMPERATURES
氢在钢中低温扩散系数 %A ZHAO Liang %A YU Gang %A ZHANG Xue-yuan %A HAN En-hou %A LIU Xiao-hui %A
赵亮 %A 余刚 %A 张学元 %A 韩恩厚 %A 刘小辉 %J 腐蚀科学与防护技术 %D 2005 %I %X The curves of hydrogen permeation in steels of A3, 08F, 16MnR and 20G were determined at temperatures between 293 K to 328 K by Devanathan-Stachurski cell. The Arrhenius equations of hydrogen diffusion coefficient versus temperature were found out. The equations may provide important fundamental parameters for monitoring the susceptivity of hydrogen induced crack while the steels are used in various industrial environments. %K hydrogen permeation %K diffusion coefficient %K low temperatures
氢渗透 %K 扩散系数 %K 低温 %U http://www.alljournals.cn/get_abstract_url.aspx?pcid=5B3AB970F71A803DEACDC0559115BFCF0A068CD97DD29835&cid=AB188D3B70B071C57EB64E395D864ECE&jid=9F6E6EC8BA5BB62698F6640073DDD6E1&aid=28AD7758CF4328F2&yid=2DD7160C83D0ACED&vid=BCA2697F357F2001&iid=94C357A881DFC066&sid=31125890FF093250&eid=381FB4265090A8E0&journal_id=1002-6495&journal_name=腐蚀科学与防护技术&referenced_num=3&reference_num=7