%0 Journal Article %T TENSILE PROPERTIES AND MICROSTRUCTURE OF AGED Ti-6Al-4V ALLOY SUBJECTED TO CYCLIC TEMPERATURE FIELD
循环温度场作用下时效态TC4合金的拉伸性能及组织 %A GENG Hongbin %A HE Shiyu %A LEI Tingquan %A
耿洪滨 %A 何世禹 %A 雷廷权 %J 材料研究学报 %D 1997 %I %X The thermal cycling tests between 77 and 623K were performed on the aged Ti-6Al-4V alloy and the tensile properties before and after thermal cycling were evaluated. The results show that the strength of the near-peak-aged alloy decreases and that of the over-aged changes little after 1000 thermal cycles. The ductility decreases and the dislocation density or amount of deformation twins and stacking faulty in the alloy increase after thermal cycling. The dominantly activated slip systems by thermal stress in 2 are {O110}2110], and the activated twins are{1011}. %K titanium alloy thermal cycling tensile property microstructure
钛合金 %K 热循环 %K 拉伸性能 %K 显微组织 %U http://www.alljournals.cn/get_abstract_url.aspx?pcid=5B3AB970F71A803DEACDC0559115BFCF0A068CD97DD29835&cid=84529CA2B2E519AC&jid=C101C4C04993B4D94FCD8446E6CBEB3B&aid=6FA7108B040863FC&yid=5370399DC954B911&vid=708DD6B15D2464E8&iid=E158A972A605785F&sid=BFB86B6ED3A99B9D&eid=6B3068A7C27BD349&journal_id=1005-3093&journal_name=材料研究学报&referenced_num=0&reference_num=6