%0 Journal Article %T Studies on the Crystallization Dynamics of Ca-P-Si Glass-Ceramic
TiO2对CaO-MgO-P2O5-SiO2系玻璃晶化影响的研究 %A YU Bing %A LIANG Kai-Ming %A GU Shou-Ren %A
俞冰 %A 梁开明 %A 顾守仁 %J 无机材料学报 %D 2002 %I Science Press %X CaO-MgO-P2O5-SiO2 glass-ceramic is a new medicinal biologic material. It not only has good biocompatibility but also improves mechanical properties. The kinetic parameters of this glass-ceramic were calculated by differential thermal analysis (DTA) and the JMA equation. The results indicate that the content of TiO2 effects on the crystallization activation energy (E) and the crystal growth index (n). E increases with the increasing of TiO2 content. And E reaches a max value when TiO2 content is about 8.7%. When TiO2 content increases further (>8.7%), E decreases inversely. The rule of n vs TiO2 content is consistent with that of E vs TiO2 content. %K biologic glass-ceramic %K crystallization %K ceramic restorations
TiO2 %K CaO-MgO-P2O5-SiO2系玻璃 %K 晶化 %K 生物微晶玻璃 %K 析晶 %K 差热分析 %K 氧化钙 %K 氧化镁 %K 五氧化二磷 %K 生物材料 %K 二氧化钛 %K 二氧化硅 %U http://www.alljournals.cn/get_abstract_url.aspx?pcid=5B3AB970F71A803DEACDC0559115BFCF0A068CD97DD29835&cid=84529CA2B2E519AC&jid=ABC0063016AF57E1C73EF43C8D2212BD&aid=176E10500DC3C9AD&yid=C3ACC247184A22C1&vid=BCA2697F357F2001&iid=38B194292C032A66&sid=47F7649551A37CFC&eid=FE6B7E9BDCCDBAA6&journal_id=1000-324X&journal_name=无机材料学报&referenced_num=3&reference_num=14